Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.00 - 8.00 µm/m-°C @Temperature 20.0 - 200 °C |
3.33 - 4.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |