Polymer Property : CTE, linear = 4.39 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.39 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-BAK4 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.90 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.39 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SF5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.90 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.39 µin/in-°F

@Temperature -22.0 - 158 °F
Schott SF56A Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.90 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.39 µin/in-°F

@Temperature -22.0 - 158 °F
Schott UG1 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 7.90 µm/m-°C

@Temperature 25.0 - 800 °C
4.39 µin/in-°F

@Temperature 77.0 - 1470 °F
ASTM-C372
CoorsTek ADS-96R 96% Alumina Thick Film Substrate
This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers
CTE, linear 7.90 µm/m-°C

@Temperature 25.0 - 800 °C
4.39 µin/in-°F

@Temperature 77.0 - 1470 °F
ASTM-C372
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film
Applications: thick films and lasers
CTE, linear 7.90 µm/m-°C

@Temperature 25.0 - 800 °C
4.39 µin/in-°F

@Temperature 77.0 - 1470 °F
ASTM-C372
CoorsTek Superstrate® 996 99.6% Alumina Thin Film
Applications: thin film substrates
CTE, linear 7.90 µm/m-°C

@Temperature 25.0 - 800 °C
4.39 µin/in-°F

@Temperature 77.0 - 1470 °F
ASTM-C372
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film
Applications: thin film substrates
CTE, linear 7.90 µm/m-°C

@Temperature 30.0 - 800 °C
4.39 µin/in-°F

@Temperature 86.0 - 1470 °F
Ametek Molybdenum-Copper Composite AMC 8020
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..
CTE, linear 7.90 µm/m-°C

@Temperature 20.0 - 600 °C
4.39 µin/in-°F

@Temperature 68.0 - 1110 °F
Advanced Ceramics ACL 1085 (C-795) Alumina
Information provided by Advanced Ceramics Limited (ACL)