Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.70 µm/m-°C @Temperature 25.0 - 500 °C |
4.28 µin/in-°F @Temperature 77.0 - 932 °F |
|
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG4 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GG420 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG385, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 300 °C |
4.28 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF31a Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 1000 °C |
4.28 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Advanced Ceramics ALC 1082 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 25.0 - 260 °C |
4.28 µin/in-°F @Temperature 77.0 - 500 °F |
|
Carpenter Pyromet® CTX-3 Superalloy, Heat Treated Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 25.0 - 260 °C |
4.28 µin/in-°F @Temperature 77.0 - 500 °F |
|
Carpenter Pyromet® CTX-3 Superalloy, Heat Treatment for Brazing Cycles over 982°C Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 25.0 - 204 °C |
4.28 µin/in-°F @Temperature 77.0 - 399 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 800 °C |
4.28 µin/in-°F @Temperature 68.0 - 1470 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 1000 °C |
4.28 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Advanced Ceramics ALC 1081 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 600 °C |
4.28 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec 848 Zirconia, ZrO2•MgO Tetragonal zirconia exhibits high flexural strength and superior low temperature stability. It features higher impact strength and erosive wear resistance as compared to alumina. 848 TTZP (yellow) i.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GG400 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG385, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 600 °C |
4.28 µin/in-°F @Temperature 68.0 - 1110 °F |
|
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
CTE, linear | 7.70 µm/m-°C @Temperature 20.0 - 600 °C |
4.28 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN EN 821-1 |
CeramTec Rubalit® IS 95 Brown Alumina Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at.. |