Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck WCu 85/15 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BAK1 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SK11 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 - 400 °C |
4.22 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 - 200 °C |
4.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume productio.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 25.0 - 800 °C |
4.22 µin/in-°F @Temperature 77.0 - 1470 °F |
ASTM-C372 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 371 °C |
4.22 µin/in-°F @Temperature 700 °F |
|
Carpenter Invar 36® Alloy, Annealed Bars and Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 371 °C |
4.22 µin/in-°F @Temperature 700 °F |
|
Carpenter Invar 36® Alloy, Cold Drawn Bars Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 371 °C |
4.22 µin/in-°F @Temperature 700 °F |
|
Carpenter Invar 36® Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK12 Glass Information Provided by SCHOTT North America, Inc. |