CTE, linear 374 µm/m-°C

@Temperature 250 - 260 °C
208 µin/in-°F

@Temperature 482 - 500 °F
Z-Axis, Alpha 2; IPC-TM-650.2.4.41
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..