Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 370 µm/m-°C @Temperature 85.0 °C |
206 µin/in-°F @Temperature 185 °F |
|
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |