Polymer Property : CTE, linear = 302 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 543 µm/m-°C

@Temperature 100 - 120 °C
302 µin/in-°F

@Temperature 212 - 248 °F
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating
3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri..