Thermal Properties Metric English Comments
CTE, linear 7.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott WG320 Long Pass Filter
Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66..
CTE, linear 7.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BASF2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BK7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAK7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.10 µm/m-°C

@Temperature 20.0 - 300 °C
3.94 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SK2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.10 µm/m-°C

@Temperature 20.0 - 300 °C
3.94 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAF21 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.10 µm/m-°C

@Temperature 20.0 - 400 °C
3.94 µin/in-°F

@Temperature 68.0 - 752 °F
DIN EN 821-1
CeramTec Rubalit® IS 95 Alumina
Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva..
CTE, linear 7.10 µm/m-°C

@Temperature 20.0 - 200 °C
3.94 µin/in-°F

@Temperature 68.0 - 392 °F
Advanced Ceramics ACL 1091 (C-799) Alumina
Information provided by Advanced Ceramics Limited (ACL)