Thermal Properties Metric English Comments
CTE, linear 3.24 µm/m-°C

@Temperature 20.0 - 400 °C
1.80 µin/in-°F

@Temperature 68.0 - 752 °F
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o..
CTE, linear 3.24 µm/m-°C

@Temperature 20.0 - 500 °C
1.80 µin/in-°F

@Temperature 68.0 - 932 °F
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o..