Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 450 °C |
3.22 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1760 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 450 °C |
3.22 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 300 °C |
3.22 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1751 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BK10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LASF40 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SSK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAF34 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK33A Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK34 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 25.0 - 800 °C |
3.22 µin/in-°F @Temperature 77.0 - 1470 °F |
|
CoorsTek ACI-Co10 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 25.0 - 800 °C |
3.22 µin/in-°F @Temperature 77.0 - 1470 °F |
|
CoorsTek ACI-Ni6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 800 °C |
3.22 µin/in-°F @Temperature 68.0 - 1470 °F |
|
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |