Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.10 µm/m-°C @Temperature 20.0 - 700 °C |
1.72 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Zircar Refractory Composites ZIRCAL-18 Refractory Board Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m.. |
|||
CTE, linear | 3.10 µm/m-°C @Temperature 20.0 - 700 °C |
1.72 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Zircar Refractory Composites ZIRCAL-45 Refractory Board Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com.. |
|||
CTE, linear | 3.10 µm/m-°C @Temperature 20.0 - 700 °C |
1.72 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |