Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 100 °C |
3.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1750 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 100 °C |
3.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1760 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 300 °C |
3.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1801 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 450 °C |
3.06 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck HPM 1810 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 100 °C |
3.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck HPM 1750 Tungsten High Density Composite Sheet Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the custo.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LASF43 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 °C |
3.06 µin/in-°F @Temperature 68.0 °F |
|
Zircar Refractory Composites ZIRCAL-18 Refractory Board Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 °C |
3.06 µin/in-°F @Temperature 68.0 °F |
|
Zircar Refractory Composites ZIRCAL-45 Refractory Board Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 °C |
3.06 µin/in-°F @Temperature 68.0 °F |
|
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 25.0 - 400 °C |
3.06 µin/in-°F @Temperature 77.0 - 752 °F |
|
CoorsTek ACI-Co10 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
CTE, linear | 5.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAK14 Glass Information Provided by SCHOTT North America, Inc. |