Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 287.6 µm/m-°C @Temperature 120 °C |
159.8 µin/in-°F @Temperature 248 °F |
Z direction |
CRP Technology Windform® XT Polyamide-Carbon Composite WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with .. |