Polymer Property : CTE, linear = 230.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 230.7 µm/m-°C

@Temperature 80.0 °C
128.2 µin/in-°F

@Temperature 176 °F
Z direction
CRP Technology Windform® XT Polyamide-Carbon Composite
WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with ..