Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 22.7 - 23.7 µm/m-°C @Temperature 20.0 - 200 °C |
12.6 - 13.2 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |