Thermal Properties Metric English Comments
CTE, linear 225 µm/m-°C

@Temperature 20.0 °C
125 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; Perkin Elmer TMS-2
Aptek 6109-A/B Epoxy Encapsulant
Optoelectronic grade flexible water clear encapsulant. Higher viscosity/lower Tg version for clear blob-top encapsulation of ceramic substrate devicesPart A is blue. Part B is clear to pale yellow.I..