Polymer Property : CTE, linear = 22.1 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 22.1 µm/m-°C

@Temperature 20.0 °C
12.3 µin/in-°F

@Temperature 68.0 °F
Across Surface; ASTM D-696
Glastic GLASTHERM HT200 Insulation Sheet
HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas..
CTE, linear 22.1 µm/m-°C

@Temperature 20.0 °C
12.3 µin/in-°F

@Temperature 68.0 °F
Across Surface; ASTM D-696
Glastic GLASTHERM HT Insulation Sheet
Glastherm Grade HT is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT is completely as..