Polymer Property : CTE, linear = 2.30 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 2.30 µm/m-°C

@Temperature 25.0 - 300 °C
1.28 µin/in-°F

@Temperature 77.0 - 572 °F
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2)
Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America.