Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 194 µm/m-°C @Temperature >=60.0 °C |
108 µin/in-°F @Temperature >=140 °F |
above Tg |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |
|||
CTE, linear | 194 µm/m-°C @Temperature >=60.0 °C |
108 µin/in-°F @Temperature >=140 °F |
above Tg |
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett.. |