Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 178 µm/m-°C @Temperature 200 - 300 °C |
99.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ TR 1105 PTFE
(discontinued **) Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne.. |