Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.02 µm/m-°C @Temperature 300 °C |
9.456 µin/in-°F @Temperature 572 °F |
0.100-in Cold-Rolled Plate; ASTM E 228 |
Special Metals INCOLOY® alloy 832 Stainless Steel INCOLOY® alloy 832 is a low cost stainless steel developed specifically for domestic and industrial sheathed heater applications. With specific chemistry additions to ensure satisfactory formula.. |