Polymer Property : CTE, linear = 16.8 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 16.8 µm/m-°C

@Temperature 25.0 - 500 °C
9.33 µin/in-°F

@Temperature 77.0 - 932 °F
Osprey Metals CE17 Al-Si Controlled Expansion Alloy
Al-27%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
CTE, linear 16.8 µm/m-°C

@Temperature 25.0 - 500 °C
9.33 µin/in-°F

@Temperature 77.0 - 932 °F
Osprey Metals CE17M Al-Si Controlled Expansion Alloy
Al-27%Si+ controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
CTE, linear 16.8 µm/m-°C

@Temperature 400 °C
9.33 µin/in-°F

@Temperature 752 °F
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 900 °C
9.33 µin/in-°F

@Temperature 68.0 - 1650 °F
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..
CTE, linear 16.8 µm/m-°C

@Temperature 427 °C
9.33 µin/in-°F

@Temperature 801 °F
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel
INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd..
CTE, linear 16.8 µm/m-°C

@Temperature 700 °C
9.33 µin/in-°F

@Temperature 1290 °F
Special Metals INCOLOY® alloy 864
INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum 440A Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 649°C (1200°F) Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Annealed
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 204°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 427°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 482°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 600 °C
9.33 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 538°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..
CTE, linear 16.8 µm/m-°C

@Temperature 21.0 - 982 °C
9.33 µin/in-°F

@Temperature 69.8 - 1800 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include ..