Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.74 µm/m-°C @Temperature 900 °C |
9.300 µin/in-°F @Temperature 1650 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |