Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 130 - 150 µm/m-°C @Temperature 25.0 - 300 °C |
72.2 - 83.3 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM D696 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |