Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 27.0 µm/m-°C @Temperature <=100 °C |
15.0 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature -30.0 - 0.000 °C |
15.0 µin/in-°F @Temperature -22.0 - 32.0 °F |
longitudinal direction, 100 x 15 x 3 mm sample; AZDEL Test |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |
|||
CTE, linear | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; Perkin Elmer TMS-2 |
Aptek 6550-A/B Epoxy Encapsulant High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for.. |