Thermal Properties Metric English Comments
CTE, linear 148 µm/m-°C

@Temperature 50.0 - 100 °C
82.2 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
DSM Somos® WaterClear® 10120 Epoxy Resin for Stereolithography  (discontinued **)
DescriptionDSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us..
CTE, linear 148 µm/m-°C

@Temperature >=149 °C
82.0 µin/in-°F

@Temperature >=300 °F
ASTM E228
Greene Tweed Arlon® 1330 PEEK
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..