Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.69 µm/m-°C @Temperature 25.0 - 100 °C |
8.161 µin/in-°F @Temperature 77.0 - 212 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
CTE, linear | 14.69 µm/m-°C @Temperature 25.0 - 100 °C |
8.161 µin/in-°F @Temperature 77.0 - 212 °F |
|
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
CTE, linear | 14.69 µm/m-°C @Temperature 25.0 - 100 °C |
8.161 µin/in-°F @Temperature 77.0 - 212 °F |
|
Carpenter 20Cb-3® Stainless Steel, Strip, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |