Thermal Properties Metric English Comments
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4..
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 20% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 25% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
CTE, linear 14.19 µm/m-°C

@Temperature 25.0 - 50.0 °C
7.883 µin/in-°F

@Temperature 77.0 - 122 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 30% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..