Polymer Property : CTE, linear = 133 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 133 µm/m-°C

@Temperature 90.0 - 150 °C
73.9 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Proto3000 Accura® Amethyst™ Material for use with Viper™ SLA® systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. FEATURES:Outstanding accuracyExceptional detailHigh thermal resistanceDeep purple colorLow as..
CTE, linear 133 µm/m-°C

@Temperature 90.0 - 150 °C
73.9 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing..