Thermal Properties Metric English Comments
CTE, linear 110 - 120 µm/m-°C

@Temperature 25.0 - 200 °C
61.1 - 66.7 µin/in-°F

@Temperature 77.0 - 392 °F
ASTM D696
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...