Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.87 µm/m-°C @Temperature 29.0 - 538 °C |
7.150 µin/in-°F @Temperature 84.2 - 1000 °F |
|
Kennametal Stellite Stellite® 33 Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-o.. |