Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.8 - 22.8 µm/m-°C @Temperature 20.0 - 100 °C |
12.1 - 12.7 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 21.8 - 22.8 µm/m-°C @Temperature 20.0 - 100 °C |
12.1 - 12.7 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |