CTE, linear 11.32 µm/m-°C

@Temperature 21.0 - 427 °C
6.289 µin/in-°F

@Temperature 69.8 - 801 °F
Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360)
TLS 17-4 is a precipitation hardening, martensitic stainless steel that exhibits excellent resistance to atmospheric and chemical corrosion. TLS 17-4 exhibits an excellent combination of high stren..