Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG34 Conversion Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include FG3, FG13 |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott OG590 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, GG385, RG610, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG610 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, GG385, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG645 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG665 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG695 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG830 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG850 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 300 °C |
5.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG9 Band Pass Filter Colloidally/ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 21.0 - 93.0 °C |
5.94 µin/in-°F @Temperature 69.8 - 199 °F |
|
Crucible Steel CPM® 10V® (AISI A11) Tool Steel CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.94 µin/in-°F @Temperature 68.0 - 199 °F |
|
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 25.0 - 50.0 °C |
5.94 µin/in-°F @Temperature 77.0 - 122 °F |
|
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 100 °C |
5.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carpenter No. 484® (Carpenter Air-Hard; AISI A2) No. 484 tool steel is an air hardening steel capable of hardening throughout in heavy sections. It has been used for those applications in which the sections are very large and those involving extre.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 25.0 - 50.0 °C |
5.94 µin/in-°F @Temperature 77.0 - 122 °F |
|
Carpenter Chrome Core® 12-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 100 °C |
5.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carpenter Hampden® High Carbon, High Chrome Tool Steel (Oil-Wear) (AISI D3) Hampden tool steel is an oil-hardening, high-carbon, high-chromium die steel having extreme wear resistance, It hardens with very little change in size or shape. Hampden tool steel is a deep-hardeni.. |
|||
CTE, linear | 10.7 µm/m-°C @Temperature 20.0 - 150 °C |
5.94 µin/in-°F @Temperature 68.0 - 302 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |