Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.60 µm/m-°C @Temperature 25.0 °C |
5.889 µin/in-°F @Temperature 77.0 °F |
|
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |