Thermal Properties Metric English Comments
CTE, linear 0.600 µm/m-°C

@Temperature 500 °C
0.333 µin/in-°F

@Temperature 932 °F
Momentive Performance Materials Type 214 Fused Quartz Tubing
Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo..
CTE, linear 0.600 µm/m-°C

@Temperature 500 °C
0.333 µin/in-°F

@Temperature 932 °F
Momentive Performance Materials Type 219 Fused Quartz Tubing
Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran..
CTE, linear 0.600 µm/m-°C

@Temperature 500 °C
0.333 µin/in-°F

@Temperature 932 °F
Momentive Performance Materials Type 254 Fused Quartz Tubing
A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen ..
CTE, linear 0.600 µm/m-°C

@Temperature 20.0 - 300 °C
0.333 µin/in-°F

@Temperature 68.0 - 572 °F
Schott LITHOSIL-Q Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 0.600 µm/m-°C

@Temperature 20.0 - 200 °C
0.333 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Sikor® E Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
CTE, linear 0.600 µm/m-°C

@Temperature 20.0 - 200 °C
0.333 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..