Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.496 µm/m-°C @Temperature 44.0 - 116 °C |
0.276 µin/in-°F @Temperature 111 - 241 °F |
|
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |