Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.465 µm/m-°C @Temperature -40.0 - 44.0 °C |
0.258 µin/in-°F @Temperature -40.0 - 111 °F |
|
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |