Polymer Property : CTE, linear = -1.11 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear -2.00 µm/m-°C

@Temperature 0.000 - 250 °C
-1.11 µin/in-°F

@Temperature 32.0 - 482 °F
average, in "a" direction
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..