Thermal Properties | Metric | English | Comments |
---|---|---|---|
Active Range | 100 - 250 °C | 212 - 482 °F | |
Indium Corp. Indalloy® 84004 Flux #4-0A Clear Liquid Flux Indalloy Flux #4-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains o.. |