Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 98.5 µm/m-°C @Temperature -30.0 - 30.0 °C |
54.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36L PA6.12 LNP* LUBRICOMP* IFL36L is a compound based on Nylon 6/12 containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Low Extractable, Wear Resistant. |