Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 97.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
54.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |