Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 97.7 µm/m-°C

@Temperature -30.0 - 30.0 °C
54.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP
LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable.