Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 92.6 µm/m-°C @Temperature -30.0 - 30.0 °C |
51.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06483 PA 46 LNP* Lubricomp* 9X06483 is a compound based on a Nylon 4/6 containing PTFE. Added feature of this grade is: Heat Stabilized. |