Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 8.80 µm/m-°C @Temperature 23.0 °C |
4.89 µin/in-°F @Temperature 73.4 °F |
|
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |