Polymer Property : CTE, linear, Transverse to Flow = 76.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 76.7 µm/m-°C

@Temperature -40.0 - 40.0 °C
42.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DX09407H PC
LNP* LUBRICOMP* DX09407H is a compound based on High Heat Polycarbonate containing proprietary fillers. Added features of this grade are: Wear Resistant, Healthcare.