Polymer Property : CTE, linear, Transverse to Flow = 74.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 74.7 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.5 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP VERTON RV00AE PA 66
LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural.