Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 70.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the .. |
|||
CTE, linear, Transverse to Flow | 70.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |