Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 68.5 µm/m-°C @Temperature -30.0 - 30.0 °C |
38.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant |