Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 65.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |